MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Iran Petrochemical (PCC) 2404TC47 Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: LDPE 2404TC47 Light duty Film
It is used for very thin films requiring good optical properties for general packaging applications e.g. covering film with very low blocking tendency.

Information provided by Iran Petrochemical Commercial Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.924 g/ccISO 1183
Melt Flow 4.7 g/10 minISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 13.0 MPaISO R527-1
Film Tensile Strength at Yield, TD 13.0 MPaISO R527-1
Film Elongation at Break, MD 100 %ISO R527-1
Film Elongation at Break, TD >= 450 %ISO R527-1
Modulus of Elasticity 0.230 GPaMD; ISO R527-1
 0.250 GPaTD; ISO R527-1
Tensile Impact 130 J/cmASTM D4272
Coefficient of Friction 0.20ASTM D1894
Tear Strength 30.0 kN/mTD; ISO 6383-2
 90.0 kN/mMD; ISO 6383-2
Film Tensile Strength at Break, MD 27.0 MPaISO R527-1
Film Tensile Strength at Break, TD 16.0 MPaISO R527-1
 
Optical PropertiesOriginal ValueComments
Haze 12 %ASTM D1003A
Gloss 50 %ASTM D2457
 
Descriptive Properties
Clarity, mV28Sabtec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) 09X02 Linear Low Density Polyethylene
Iran Petrochemical (PCC) 12XF6 Linear Low Density Polyethylene
Iran Petrochemical (PCC) 1922T Low Density Polyethylene
Iran Petrochemical (PCC) 2102TX00 Low Density Polyethylene
Iran Petrochemical (PCC) 2101TN47 Low Density Polyethylene

PIPC260 / 149722

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.