Bayhydrol AH XP 2741 is an aqueous core-shell styrene acrylate dispersion. Properties / Applications: Bayhydrol AH XP 2741 is a primary styrene acrylic dispersion to formulate one-component clear and pigmented primers and topcoats. Coatings based on Bayhydrol AH XP 2741 show very good chemical resistance and high film hardness. This product can be combined with polyurethane dispersions or other acrylic dispersions, after checking the specific product compatibility. Bayhydrol AH XP 2741 is specially recommended for wood coatings applications. As with any product, use of Bayhydrol AH XP 2741 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability. Information provided by Covestro |