MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) KetaSpire® KT-880 CF30 PEEK, 30% carbon fiber
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: 30% carbon fiber, high melt flow for injection molding

KetaSpire® KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanical properties at temperatures approaching 300°C and the lowest coefficient of linear thermal expansion within the KetaSpire® product family.

KetaSpire® PEEK is produced to the highest industry standards and is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, ease of melt processing, high purity and excellent chemical resistance to organics, acids and bases.

These properties make it well-suited for applications in healthcare, transportation, electronics, chemical processing and other industrial uses.

Markets/Uses: Aircraft / Mechanical & Structural Applications / Brackets and Hinges; Aircraft / Mechanical & Structural Applications / Engine Components; Aircraft / Mechanical & Structural Applications / Environmental Control System Components; Aircraft / Mechanical & Structural Applications / Mounting Support Rails; Aircraft / Mechanical & Structural Applications / Seals; Aircraft / Mechanical & Structural Applications / Spuds; Aircraft / Mechanical & Structural Applications / Stock Shapes for Prototyping; Aircraft / Mechanical & Structural Applications / Support Brackets; Aircraft / Mechanical & Structural Applications / Threaded Fasteners; Films / High Temperature Films / Brackets and Hinges; Films / High Temperature Films / Engine Components; Films / High Temperature Films / Environmental Control System Components; Films / High Temperature Films / Mounting Support Rails; Films / High Temperature Films / Seals; Films / High Temperature Films / Spuds; Films / High Temperature Films / Threaded Fasteners; Healthcare / Medical Devices / Medical Pump Seals; Healthcare / Medical Devices / Medical Reusable; Healthcare / Medical Devices / Medical/Healthcare Applications; Healthcare / Medical Devices / Orthopedics; Healthcare / Medical Devices / Packaging, Rigid Medical; Healthcare / Medical Devices / Surgical Instruments; Miscellaneous / Industrial / Compressor Components; Oil & Gas / Down Hole / Back-Up Seal Rings; Oil & Gas / Down Hole / Compressor Components; Oil & Gas / Down Hole / Compressor Plates; Oil & Gas / Down Hole / Down Hole Connectors; Oil & Gas / Down Hole / Electrical Connectors; Oil & Gas / Down Hole / Poppets

Applications: Aircraft Applications; Connectors; Dental Applications; Electrical/Electronic Applications; Film; Hospital Goods; Industrial Applications; Medical Devices; Medical/Healthcare Applications; Oil/Gas Applications; Pump Parts; Seals; Surgical Instruments

Features: Autoclave Sterilizable; Chemical Resistant; E-beam Sterilizable; Ethylene Oxide Sterilizable; Fatigue Resistant; Flame Retardant; Good Dimensional Stability; Good Sterilizability; Heat Sterilizable; High Flow; High Heat Resistance; High Stiffness; High Strength; Radiation (Gamma) Resistant; Radiation Sterilizable; Radiotranslucent; Steam Resistant; Steam Sterilizable

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccASTM D792
Water Absorption 0.10 %
@Time 86400 sec
ASTM D570
Viscosity 450 cP
@Shear Rate 1000 1/s,
Temperature 400 °C
Melt; ASTM D3835
Linear Mold Shrinkage, Flow <= 0.0020 cm/cm
@Thickness 3.18 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.014 - 0.016 cm/cm
@Thickness 3.18 mm
ASTM D955
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 400 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 106ASTM D785
Tensile Strength 223 MPaASTM D638
Tensile Strength, Yield 218 MPaType 1A, 5 mm/min; ISO 527-2
Elongation at Break 1.7 %5.0 mm/min; ASTM D638
 1.7 %Type 1A, 5 mm/min; ISO 527-2
Tensile Modulus 20900 MPaASTM D638
 25400 MPa1 mm/min, Type 1A; ISO 527-2
Flexural Strength 319 MPaISO 178
 321 MPaASTM D790
Flexural Modulus 17900 MPaASTM D790
 21500 MPaISO 178
Compressive Strength 188 MPaASTM D695
Shear Strength 103 MPaASTM D732
Izod Impact, Notched 64.0 J/mASTM D256
Izod Impact, Unnotched 640 J/mASTM D256
Izod Impact, Notched (ISO) 8.50 kJ/m²ISO 180
Izod Impact, Unnotched (ISO) 43.0 kJ/m²ISO 180
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 6.70 µm/m-°C
@Temperature -50.0 - 50.0 °C
ASTM E831
Specific Heat Capacity 1.31 J/g-°C
@Temperature 50.0 °C
ASTM C351
 1.81 J/g-°C
@Temperature 200 °C
ASTM C351
Thermal Conductivity 0.370 W/m-KASTM C177
Melting Point 343 °CPeak; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 315 °CAnnealed; ASTM D648
Glass Transition Temp, Tg 147 °CDSC
Flammability, UL94 V-0
@Thickness 0.800 mm
 V-0
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 365 °C
Middle Barrel Temperature 370 °C
Front Barrel Temperature 375 °C
Nozzle Temperature 380 °C
Mold Temperature 175 - 205 °C
Drying Temperature 150 °C
@Time 14400 sec
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
Injection RateFast
ProcessingInjection Molding; Machining; Profile Extrusion
Screw Compression Ratio2.5:1.0 to 3.5:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4335 / 280135

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.