Product: PLEXIGLAS® Film 0F011 is a transparent, glossy and high weather resistant acrylic film for outdoor applications. Due to its superior performance under long term weathering and UV light exposure, PLEXIGLAS® Film 0F011 does not present color change or yellowing. Therefore it provides an enhanced protection of plastic substrates from degradation caused by UV wave lengths. Application: PLEXIGLAS® Film 0F011 is suitable as top layer for high UV and weathering protection of polymeric substrates, especially for PVC decoration films. The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm). |