MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® 1015CR PA6, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Description: Polyamide 6, unfilled, standard for fast injection cycles, for injection molding

Available in: Asia Pacific

Product Applications: TECHNYL® 1015CR has high fluidity and a good mould release. It is particularly suitable for the production of technical moldings with fast injection cycles. This grade is used for: Fastener, Clip, Gear, Bobbin. This product is available in Natural color.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO 1183
Water Absorption 1.3 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage, Flow 0.013 - 0.020 cm/cm
Linear Mold Shrinkage, Transverse 0.015 - 0.020 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 115ASTM D786
Tensile Strength, Yield 80.0 MPaASTM D638
Elongation at Break 30 %ASTM D638
Flexural Strength 110 MPaASTM D790
Flexural Modulus 3050 MPaASTM D790
Izod Impact, Notched 65.0 J/mASTM D265
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dissipation Factor 0.020IEC 60250
Comparative Tracking Index 600 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
ISO 11359
Melting Point 222 °CISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 180 °CASTM D648
Flammability, UL94 HBISO 1210
Glow Wire Ignition Temperature 675 °C
@Thickness 0.800 mm
IEC-60695-2-13
 
Processing PropertiesOriginal ValueComments
Feed Temperature 230 - 235 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone235-345°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Samyang Trirex® 3022IR-02 Polycarbonate
Domo TECHNYL® 1021ST PA6, DRY
Domo TECHNYL® 1011R PA6, DRY
Domo TECHNYL® 1021GF6 PA6, 30% glass fiber, DRY
Plastcom SLOVAMID 6 GF 33 PA6, 33% glass fibre

PRHOD562 / 137793

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.