MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® Redux® 319A High Performance Modified Epoxy Film Adhesive (0.06 psf)
Categories: Polymer; Adhesive; Film; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Redux 319 is a high performance modified epoxy film adhesive curing at 350°F. It is available in both supported and unsupported versions at areal weights between 0.03 and 0.08 psf. The supported versions contain a woven nylon carrier for glueline thickness control and improved handleability. Redux 319 is a hot melt film which is free from solvents and consequently it has a very low volatile content.

Features: Cures in 60 min at 350°F; Good performance at temperatures ranging from -67°F to 300°F; Good short-term exposure performance at 350°F; Excellent peel properties; Good drape at ambient temperatures; Less than 1% volatile content.
Applications: Aluminum to aluminum bonding; Fiber-reinforced composite to composite bonding; Aluminum honeycomb sandwich bonding; Aramid honeycomb sandwich bonding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 2.32 ksi
@Temperature 149 °C
Lap Shear
 5.22 ksi
@Temperature 22.2 °C
Lap Shear, Primed with Redux 119
Peel Strength 38.1 pli
@Temperature 22.2 °C
Bell Peel
 
Processing PropertiesOriginal ValueComments
Shelf Life 18.0 Month
@Temperature -17.8 °C
 
Descriptive Properties
Areal Weight (psf)0.06
Climbing Drum Peel (in-lb/3in)7472°F
Standard Roll (ft2)430
SupportWoven nylon carrier

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® Redux® 319L High Performance Modified Epoxy Film Adhesive (0.036 psf)

PHEXC442 / 99261

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.