MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Americhem Engineered Compounds ColorFast® FRPBT220 PBT, Flame Retarded
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Flame Retardant

Material Notes: Super tough, flame retarded unreinforced

All information provided by LTL Color Compounders, Inc. LTL was acquired by Americhem in 2014.

Key Words: PBT
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/ccASTM D792
Linear Mold Shrinkage 0.022 in/in0.125 in.; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 124ASTM D785
Tensile Strength, Yield 5800 psi2.0 in/min; ASTM D638
Elongation at Break 145 %2.0 in/min; ASTM D638
Flexural Strength 14100 psi2.0 in/min; ASTM D790
Flexural Modulus 300000 psi2.0 in/min; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 450 - 480 °F
Middle Barrel Temperature 460 - 490 °F
Front Barrel Temperature 470 - 500 °F
Nozzle Temperature 460 - 490 °F
Melt Temperature 470 - 500 °F
Mold Temperature 120 - 170 °F
Drying Temperature 250 °F
Dry Time 3 - 4 hournominal; maximum drying time of 12 hours
Back Pressure 50.0 - 100 psi
Shot Size 40 - 60 %
Vent Depth 0.000500 - 0.00100 in
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLTLC043 / 104428

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.