MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis RA130E-2491 Polypropylene Random Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: RA130E-2491 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is blue colored. Applications: domestic water, heating, relining, plumbing, and industrial applications. The product is used for single as well as for multilayer pipes, where you then differentiate between plastic multilayer and aluminum multilayer pipes. Specifications: DIN 8078; DIN 8077; and EN ISO 15874.

Information provided by Borealis AG

Key Words: PP-R
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccISO 1183
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 25.0 MPa50mm/min; ISO 527-2
Elongation at Yield 13.5 %50mm/min; ISO 527-2
Tensile Modulus 900 MPa1mm/min; ISO 527
Flexural Modulus 800 MPa2mm/min; ISO 178
Charpy Impact Unnotched 40.0 kJ/m²
@Temperature -20.0 °C
ISO 179/1eU
 NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature 0.000 °C
ISO 179/1eU
Charpy Impact, Notched 2.00 kJ/m²
@Temperature -20.0 °C
ISO 179/1eA
 3.50 kJ/m²
@Temperature 0.000 °C
ISO 179/1eA
 20.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear 150 µm/m-°C
@Temperature 0.000 - 70.0 °C
DIN 53752
Thermal Conductivity 0.240 W/m-KDIN 52612
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 180 - 210 °Ccylinder
Die Temperature 210 - 220 °C
Melt Temperature 210 - 220 °C
Head Temperature 210 - 220 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Rigid Molding M3700
Total PPC 1645 Polypropylene, Heterophasic Copolymer, Pipes
Flint Hills P5M2Z-012 Polypropylene Random Copolymer
Borealis Bormed™ RF825MO Polypropylene Copolymer for Healthcare Applications
Borealis RE420MO Polypropylene Random Copolymer, Transparent

PBOREA558 / 108817

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.