MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Master Bond Supreme 3AOHT One Component, Thermally Conductive Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, Thermally Conductive

Material Notes: Master Bond Polymer System Supreme 3AOHT is a one component, heat cured epoxy adhesive and sealant, featuring high peel and shear strength along with excellent thermal conductivity and convenient handling. Supreme 3AOHT cures readily at 250°F in 20-30 minutes; and at 300°F in 5-10 minutes.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Storage Temperature 75.0 °F6 months
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 350 °F
Minimum Service Temperature, Air -100 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 0.0830 - 0.160 hour
@Temperature 149 °C
 0.330 - 0.500 hour
@Temperature 121 °C
 
Descriptive Properties
ColorOff-White to Light Yellow
ViscosityPasteRoom Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP42HT-2AO Two Component, Thermally Conductive, Heat Resistant Epoxy
Master Bond EP30AN Thermally Conductive Dimensionally Stable Epoxy System
Master Bond EP21TDC-2AO Flexibilized, Thermally Conductive Two Component Epoxy
Master Bond EP21TDC-2AN Two Component, Flexibilized, Highly Thermally Conductive, Electrically Insulating Epoxy Resin
Master Bond EP21TDC-2 Highly Flexible Cryogenic Epoxy Compound

PMASTB098 / 52255

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.