MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

3M Dyneon™ HC 1101 Polyetherdiamine  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: Dynamar polyetherdiamine HC 1101 is a linear polyether diprimary amine which contains tetramethylene oxide as the principal recurring unit and has a molecular weight of approximately 10000.

HC 1101 is characterized as follows

  • Primary amine and end group functionally of 2
  • High molecular weight
  • Low toxicity

HC 1101 can be utilized as the flexible reactive segment in block-type copolymer containing both flexible and rigid segments. It may be readily converted into very tough cured elastomers, for instance, by reaction with epoxy resins having an oxirane equivalence greater than one. The reaction mixtures are characteristically liquids which can be poured, cast, or molded and subsequently cured at room temperature, or more rapidly at elevated temperatures. High use levels will form elastomers characterized by the following properties:

  • High tensile strength and elongation
  • Hydrolitic stability
  • Adhesion properties similar to epoxy resins
  • Excellent abrasion resistance
  • High resilience and low heat build-up during dynamic use
  • Wide range of available hardnesses

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 2.0 %2.0 %
Melt Density 0.980 g/cc
@Temperature >=35.0 °C
0.0354 lb/in³
@Temperature >=95.0 °F
Viscosity 250000 cP
@Temperature 65.6 °C
250000 cP
@Temperature 150 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6262epoxy cured; ASTM D2240
Tensile Strength at Break 23.2 MPa3360 psiepoxy cured
Elongation at Break 340 %340 %epoxy cured
100% Modulus 2.07 MPa
@Strain 100 %
300 psi
@Strain 100 %
epoxy cured
Rebound 75 %75 %Bashore, epoxy cured
Compression Set 3.0 %3.0 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 35.0 °C95.0 °F
 
Descriptive Properties
FormWaxy Solid
Total Amine (meq./gram)0.2

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polybutadiene Rubber (BR)
BASF Isobutyleneoxide
ATG s.r.l. BR Polybutadiene Rubber

PDYNE164 / 34972

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.