MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Chesterton 752 Cold Galvanizing Compound
Categories: Fluid

Material Notes: Chesterton® 752 Cold Galvanizing Compound functions both as a zinc rich primer or final coating for ferrous metals and their welds exposed to atmospheric or corrosive conditions. The product deposits a 95% pure zinc coating that bonds to metal protecting it against corrosion both physically and by galvanic action. After fabrication or construction, it forms an all purpose protective coating. After wear, accidents, welding or maintenance work on galvanized protective coating. Chesterton 752 Cold Galvanizing Compound provides instant galvanizing. Unlike hot dip galvanizing, the product can be sprayed on to provide a convenient, fast drying protective coating.

Features:

  • 95% pure zinc in dried film
  • Ultra-fine particle size
  • Flexible
  • No heat required
  • Fast drying
  • Self healing
  • One part system
  • 3 way corrosion protection
  • Conforms to MIL-P-46105, MIL-P-21035 and MIL-P-26915
  • Authorized by the USDA

Applications: Use in maintenance and construction to restore damaged galvanized metal dn provide protection for all iron and steel surfaces, structures or equipment such as air conditioning units, agricultural machinery, automotive bodies, fences, marine equipment, metal floors and roofs, mining equipment and oil rigs, off shore drilling structures, ornamental iron works, pipe lines, railroad equipment, structural steel tanks, transmission towers, underground pipe lines, welds, ducts, marine equipment, decks etc.

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.88 g/cc
 
Mechanical PropertiesOriginal ValueComments
Impact Test 40.0 in-lbExtrusion; ASTM D2794
 >= 80.0 in-lbIntrusion; ASTM D2794
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 149 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 10.0 °CApplication Temperature
 38.0 °CApplication Temperature
Dry Time 0.250 hour
@Temperature 21.0 °C
Touch
 8.00 hour
@Temperature 21.0 °C
Recoat
 
Compliance PropertiesOriginal ValueComments
USDA Yes
 
Component Elements PropertiesOriginal ValueComments
Zinc, Zn 95 %Dried Film
 
Descriptive Properties
ColorGray
Corrosion Protection:2500 hrsASTM B117
Coverage6.6-9.8 m2/lat 0.05-0.08
DiluentXylol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chesterton ARC S1 General purpose coating

PPTCHS123 / 138235

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.