Product Description: Master Bond EP3LV represents a breakthrough in epoxy adhesive technology featuring a hitherto unattainable balance of performance properties including both high shear and high cure speed. This one component adhesive system is formulated to cure at elevated temperatures, e.g., 5-10 minutes at 300- 325°F, longer times at lower temperatures for maximum bond strengths. Tensile strengths in excess of 2000 psi are readily obtained after such short cure times. No mixing is necessary prior to use. EP3LV produces truly exceptionally good performance bonds with durable high lap shear strength for service in the remarkably wide temperature range of -100°F to +300°F. It offers superior resistance to impact, thermal shock, vibration and stress fatigue cracking while maintaining the moisture, creep, corrosion and thermal resistance typical of epoxy resin adhesives. It is 100% reactive and does not contain any diluents or solvents. EP3LV produces durable high strength, exceptionally tough bonds which are remarkable resistant to severe thermal cycling and many chemicals including water, oil, fuels and most organic solvents even upon prolonged exposures. For best results all surfaces should cleaned and then either roughened or chemically etched. Adhesion to metals, glass, ceramics, wood, vulcanized rubbers and many plastics is excellent. The hardened adhesive is a superior thermal insulator. The color is gray. EP3LV offers the convenience of a heat cure with no mixing prior to use and uniquely favorable bonding performance for even the most difficult applications in the aerospace, electronic electrical computer, metalworking, appliance, automotive and chemical industries. Product Advantages: - Single component system; no mixing prior to use. Unlimited working life at room temperature.
- Easy application; contact pressure only required during simple heat cure; adhesive spreads evenly and smoothly.
- Versatile cure schedules: 5-10 min at 300-325°F, longer time periods at lower temperatures as desired. Minimum curing temperature, 235°F.
- High tensile shear strength to similar and dissimilar substrates over the wide temperature range of -100°F to +300°F.
- Good electrical insulating properties and chemical resistance.
- Superior thermal shock; impact and stress cracking fatigue resistance.
- Superior durability and dimensional stability.
Information provided by Master Bond Inc. |
Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |