MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
3M 4000 UV 5280 Marine Adhesive/Sealant Fast Cure
Categories: Polymer; Adhesive

Material Notes: 3M™ Marine Adhesive/Sealant 4000 UV is a one-part adhesive sealant that cures to form a firm, rubbery waterproof seal. Its flexibility allows for the dissipation of stress caused by shock, vibration, swelling or shrinking. Designed for marine applications above and below the waterline. Its superior UV resistance properties makes this an ideal cosmetic adhesive sealant.

Features:

  • Superior UV resistance.
  • Non-corrosive.
  • Exceptional sealing properties.
  • Non-cracking.
  • < 1% VOC’s
  • Caulkable at low temperatures (>40°F [4°C]).
  • Low odor.
  • Fast curing.
  • Non-shrinking.
  • Paintable (test for suitability).
  • Non-sagging.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 38 - 39
Tensile Strength at Break 1.74 MPa50% RH
 2.06 MPa
@Time 3.60e+6 sec
G-26, B, BH; ASTM D412
 2.11 MPa
@Time 1.80e+6 sec
G-26, B, BH; ASTM D412
Elongation at Break 790 %50% RH
 723 %
@Time 3.60e+6 sec
G-26, B, BH; ASTM D412
 804 %
@Time 1.80e+6 sec
G-26, B, BH; ASTM D412
Shear Strength 174 psiOverlap, Teak, 50% RH
 196 psiOverlap, Teak (primed), 50% RH
 226 psiOverlap, Fir, 50% RH
 251 psiOverlap, Fiberglass, 50% RH
 279 psiOverlap, ABS, 50% RH
 329 psiOverlap, Aluminum, 50% RH
 424 psiOverlap, Gelcoat, 50% RH
 135 psi
@Time 1.80e+6 sec
Overlap, Nylon, 50% RH, Salt Water Immersion
 284 psi
@Time 1.80e+6 sec
Overlap, Fiberglass, 50% RH, Salt Water Immersion
 359 psi
@Time 1.80e+6 sec
Overlap, Gelcoat, 50% RH, Salt Water Immersion
 381 psi
@Time 1.80e+6 sec
Overlap, Aluminum, 50% RH, Salt Water Immersion
 475 psi
@Time 1.80e+6 sec
Overlap, Copper, 50% RH, Salt Water Immersion
 542 psi
@Time 1.80e+6 sec
Overlap, Bronze, 50% RH, Salt Water Immersion
 675 psi
@Time 1.80e+6 sec
Overlap, Stainless Steel, 50% RH, Salt Water Immersion
Peel Strength 5.30 pli180°, Aluminum, 50% RH
 8.00 pli180°, Teak (primed), 50% RH
 8.20 pli180°, Fiberglass, 50% RH
 8.70 pli180°, Teak, 50% RH
 8.80 pli180°, Gelcoat, 50% RH
 9.40 pli180°, Mahogany, 50% RH
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 90.0 °C
Minimum Service Temperature, Air -40.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1440 minFull Cure, 50% RH
Tack-Free Time 22.0 min50% RH
Shelf Life 12.0 Monthin the original, unopened container

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M 31U72C (Clear) Polyethylene Protective UV Tape
3M 31U26C/UV Protective UV Tape
3M 2AU23B/UV Protective UV Tape
3M 25M25X Protective UV Tape
3M 3W55Z Protective UV Tape

PMM33148 / 167895

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.