MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Daikin POLYFLON TC-7408GY PTFE Solvent-Based Coating
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Solvent-based PTFE coating for abrasion resistance with sintering at lower temperature.

Introduction: POLYFLON PTFE TC-7400 grade is a solvent-based PTFE coating; POLYFLON PTFE TC-7408GY makes a gray coating layer displaying hardness and abrasion resistance and hardness; It can be sintered at lower temperature (150 –200?)

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/cc
Solids Content 35.0 %
Viscosity Measurement 15.0[sec], Ford Cup No.4
 
Mechanical PropertiesOriginal ValueComments
Coefficient of Friction 0.0400 - 0.0800Bauden leben type, Steel ball 8mmf, Linear velocity 0.27cm/s, Loading 1.0kg
Taber Abrasion, mg/1000 Cycles 25.0 - 35.0
@Load 1.00 kg
CS-17
Abrasion 0.200 - 0.300Sliding, [mg/cm2], With SUS23B, 55.9kPa, 2.3m/s, 10 minutes
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 160 °C
 
Descriptive Properties
AppearanceGray Film
Hexadecane Contact Angle (°)35-41°
Pencil hardness3H25°C
 HAfter immersed in boiled water for 500h
Water Contact Angle (°)92-96°

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDAIK9730 / 327170

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.