MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Reltek BONDiT™ B-4811 Adhesive, Sealant & Coating System
Categories: Polymer; Adhesive; Thermoset

Material Notes: Key Properties:
  • Semi-rigid, high strength.
  • A filled version of B-481 to further increase chemical resistance and electrical properties and to lower shrinkage.
  • Ease of use.

Applications: Encapsulate sensitive instrumentation for chemical isolation, outstanding moisture resistance and ruggedness. High chemical resistance and strength. Superior for coating, priming and encapsulation in marine applications and other very harsh environments. Very easy to use and very clean two part system. Bonds to most substrates. Ambient or accelerated thermal cure.

Key Words: Epoxy Adhesive, Sealant
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 2350 psi
Elongation at Break 10 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 350 °F
Minimum Service Temperature, Air -50.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 hour
@Temperature 93.3 °C
 12.0 hour
@Temperature 22.2 °C
 
Descriptive Properties
Chemical & Moisture Resistance40=Lowest, 4=Highest

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAQREL07 / 24223

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.