MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company EMI 263 A Nylon 6 (PA); Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Antistat/Conductive; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Stainless Steel Filled

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.36 g/ccASTM D 792
Additive Loading 20 %Primary Additive
Linear Mold Shrinkage 0.0060 - 0.012 cm/cm
@Thickness 3.20 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 11200 psiASTM D 638
Elongation at Break >= 10 %ASTM D 638
Tensile Modulus 510 ksiASTM D 638
Flexural Strength 17890 psiASTM D 790
Flexural Modulus 510 ksiASTM D 790
Izod Impact, Notched 0.800 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched 21.0 ft-lb/in
@Thickness 3.20 mm
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 1.0 ohm-cmASTM D 257
Surface Resistance <= 100 ohmESD STM11.11
Surface Resistivity per Square <= 1000 ohmASTM D 257; ESD STM11.11
Static Decay <= 0.50 secFTMS101C; 4046.1
Shielding Effectiveness 87 dB
@Thickness 2.00 mm,
Frequency 5.00e+8 Hz
ASTM D 4935
 89 dB
@Thickness 2.00 mm,
Frequency 3.00e+8 Hz
ASTM D 4935
 90 dB
@Thickness 2.00 mm,
Frequency 7.00e+8 Hz
ASTM D 4935
 93 dB
@Thickness 2.00 mm,
Frequency 1e+9 Hz
ASTM D 4935
 94 dB
@Thickness 2.00 mm,
Frequency 1.30e+9 Hz
ASTM D 4935
 96 dB
@Thickness 2.00 mm,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 172 °FASTM D 648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 470 - 535 °F
Mold Temperature 130 - 200 °F
Drying Temperature 175 °F
@Time 14400 sec
Moisture Content 0.20 %
Dew Point 0.000 °F
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company EMI 262 Nylon 6/6 (PA), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company EMI 261 A Nylon 6 (PA), Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding
RTP Company RTP 2099 X 128018 B PC/PBT Alloy; Glass Fiber - Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding - (Preliminary Datasheet)
RTP Company EMI 1361 Polyphenylene Sulfide (PPS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company EMI 1262 S-80A Ester-based Thermoplastic Polyurethane Elastomer; Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding

PQZRA39590 / 205927

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.