MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
FKuR Kunststoff Eastlon® PET CB 602AB
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Eastlon Bio-PET is a partially biobased polyethylene terephthalate whose MEG content (about 30% by weight) is obtained on the basis of renewable plant raw materials. Eastlon Bio-PET is chemically identical to conventional PET and can be processed as usual to various plastic articles and subsequently recycled together with conventional PET in the existing PET recycling stream. Eastlon PET CB-602AB is particularly suitable for the production of bottles and films. Bottles made from Eastlon Bio-PET are characterized by high optical clarity as well as good resistance to a variety of chemicals and oils. Just like standard PET, Bio-PET also has a good barrier against carbon dioxide (CO2) and oxygen (O2) so it is particularly suitable for use in beverage or cosmetic packaging. The biobased carbon content (BCC) is 20%.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.820 - 0.920 g/ccISO 60
Density 1.30 - 1.40 g/ccISO 1183
Water Absorption at Saturation <= 0.40 %FENC Method
Viscosity Measurement 75 - 79Intrinsic Viscosity (ml/g); FENC Method
 
Chemical PropertiesOriginal ValueComments
Acid Value 25 - 45[meq/kg]; FENC Method
 
Thermal PropertiesOriginal ValueComments
Melting Point 240 - 260 °CISO 3146-C
 
Descriptive Properties
DEG Content (%)1.1-1.5; FENC Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ecovio® C2203 F Blend Biodegradable Polyester
Eastman Eastar GN046 Copolyester, Natural
Iran Petrochemical (PCC) PET BG-781 Polyethylene Terephthalate
Indorama StarPet Preformance® 1708 PET Resin
Global EPP PET

PFKUR940 / 192745

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.