MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Mylar® 800 Polyester Packaging Film, 48 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Data provided by DuPont Packaging Polymers.

Melinex® 800 is a clear, non-pretreated base film with high gloss, low haze and excellent processability. Melinex® 800 is available in 48 gauge. Melinex® 800 polyester film is stiffer than polypropylene and also maintains an excellent film thickness profile and roll formation to ensure consistent processability in operations. Melinex® 800 film features good clarity and handling characteristics in metallizing operations. When aluminum metallized, the film exhibits excellent aesthetic quality as well as the best barrier to oxygen and moisture in a flexible film.

Melinex® 800 is a polyester film that is compliant with the U.S. Food and Drug Administration regulations under 21 CFR 177.1630, Sections (f), (g),and (h). These sections cover the use of PET in contact with all types of foods (excluding alcoholic beverages) at temperatures up to and above 250°F (including oven baking or cooking) and alcoholic beverages (not to exceed 50 percent by alcohol by volume) at ambient temperatures.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/cc
Moisture Vapor Transmission 0.0120 cc-mm/m²-24hr-atmmetallized barrier; 2.8 g/100in²-24hr-atm unmetallized barrier; Tested per ASTM F372 at 100°F, 90% RH.
Oxygen Transmission 0.0200 cc-mm/m²-24hr-atmmetallized barrier; 6 cc/100in²-24hr-atm unmetallized barrier; Tested per ASTM D1434 at 77°F, 75% RH.
Thickness 0.480 mil
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 110 %ASTM D882A
Film Elongation at Break, TD 70 %ASTM D882A
Coefficient of Friction, Dynamic 0.40ASTM D1894
Coefficient of Friction, Static 0.50ASTM D1894
Film Tensile Strength at Break, MD 222 MPaASTM D882A
Film Tensile Strength at Break, TD 269 MPaASTM D882A
 
Optical PropertiesOriginal ValueComments
Haze 3.6 %Gardner; ASTM D1003
Transmission, Visible 88.5 %ASTM D1003
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Borseal™ TD110BF Terpolymer for BOPP Film
DuPont Teijin Films Mylar® 800C Polyester Packaging Film, 48 Gauge
DuPont Teijin Films Mylar® 840 Polyester Film, 48 Gauge
Borealis Borseal™ TD115BF Terpolymer for BOPP Film
DuPont Teijin Films Mylar® 800C Polyester Packaging Film, 75 Gauge

PDU7A3 / 33193

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.