MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kureha KF Polymer 850 PVDF Homopolymer
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF polymer is being used in applications where heat resistance, anticorrosion, and weather-resistance are important.

Typical Applications:

  • Chemical valves, Pump part, & Fittings
  • Binder for lithium ion batteries
  • Hollow fiber for filtration of city water and sewage
  • Film & Sheet

Information provided by Kureha.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.77 - 1.79 g/ccASTM D792
Viscosity 1200 cP
@Shear Rate 50 1/s,
Temperature 240 °C
Melt; ASTM D3835
Viscosity Test 0.85 cm³/g
@Temperature 30.0 °C
Inherent Viscosity in DMF Solution
Melt Flow 18 - 26 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 57.0 MPaISO 527-2
Elongation at Break 76 %ISO 527-2
Tensile Modulus 2.51 GPaISO 527-2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1e+15 - 1e+16 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
Melting Point 173 °CASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °CISO 75-2
Flammability, UL94 V-0
@Thickness 1.47 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
VICTREX™ PEEK 450G™ General Purpose
Arkema Kynar® 720 Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion
Kureha KF Polymer 1000 PVDF Homopolymer
RTP Company RTP 3300 Polyvinylidene Fluoride (PVDF) Base Resin
Techmer ES HiFill® TPX-PVDF-03009 C

PKUREHA90 / 150354

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.