MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayhydur® 303 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Bayhydur 303 is a solvent-free, water-dispersible polyisocyanate resin based on hexamethylene diisocyanate (HDI).

Properties / Applications: Bayhydur 303 polyisocyanate is a solvent-free, water-dispersible crosslinking agent for hydroxyl- function waterborne resins. It is dispersed in the aqueous resin by direct addition and simple agitation, just prior to use. Reaction occurs under ambient conditions. The pot life varies with the aqueous resin used, but can be several hours in duration. After the polyisocyanate has been added to the waterborne component, the container should not be hermetically sealed, since a pressure buildup may occur due to carbon dioxide formation. As with any product, use of Bayhydur 303 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/cc
Viscosity 1600 - 3200 cP1600 - 3200 cP
 
Thermal PropertiesMetricEnglishComments
Flash Point 178 °C352 °FSetaflash
 
Descriptive Properties
AppearancePale, yellow viscous liquid
Content<0.2%Monomer
 18.8-19.8%NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOVEST0191 / 201974

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.