MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Telcar® TL-1934E Styrenic Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE; Vinyl (PVC); PVC, Wire and Cable Grade

Material Notes: Notes: Telcar TL-1934E is a general purpose thermoplastic elastomer designed for electrical applications requiring flexibility over a wide temperature range. Telcar TL-1934E is a high hardness, high density grade that is UL 94 rated with 720hr sunlight resistance. This grade is suitable for both injection molding and extrusion.

Features: Brominated; Flame Retardant; General Purpose; Good Colorability; Good Flexibility; Halogenated; High Hardness; High Specific Gravity; Low Flow; Slip; Sunlight Resistant (720 hrs); UV Resistant

Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Core Insulation; Wire & Cable Application; Wire Jacketing

Form: Pellets

Processing Method: Injection Molding; Extrusion

Injection Notes: Injection Rate: Moderate-Fast

Extrusion Notes: Screw Speed: 30 to 100 rpm

Information Provided by Teknor Apex

Key Words: TES
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccASTM D792
Melt Flow 18 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 83ASTM D2240
Tensile Strength at Break 1246.0 psiChange in tensile strength in air after 168 hours at 316°F; ASTM D573
 1344 psiChange in tensile strength in air after 3600 hours at 268°F; ASTM D573
 1400 psi20 in/min; ASTM D412
 8.50 MPa
@Treatment Temp. 60.0 °C,
Time 605000 sec
in IRM 902 Oil; ASTM D471
 9.65 MPa
@Treatment Temp. 136 °C,
Time 605000 sec
in Air; ASTM D573
Elongation at Break 462.0 %After aging in air 3600 hours at 268°F; ASTM D573
 467.5 %After aging in air 168 hours at 316°F; ASTM D573
 550 %20 in/min; ASTM D412
 495 %
@Treatment Temp. 136 °C,
Time 605000 sec
in Air; ASTM D471
 495 %
@Treatment Temp. 60.0 °C,
Time 605000 sec
in IRM 902 Oil; ASTM D471
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.4ASTM D150
Dielectric Strength 900 V/milASTM D419
Dissipation Factor 0.0040ASTM D150
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 221 °FContinuous; UL 1581
Brittleness Temperature -74.2 °FASTM D746
UL RTI, Electrical 122 °FUL 746
UL RTI, Mechanical with Impact 122 °FUL 746
Flammability, UL94 V-0
@Thickness 1.52 mm
QMFZ2.E54709; QMTT2.E73402
Oxygen Index 26 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 340 - 380 °F
Middle Barrel Temperature 350 - 390 °F
Front Barrel Temperature 360 - 400 °F
Nozzle Temperature 370 - 410 °F
Zone 1 330 - 370 °F
Zone 2 340 - 380 °F
Zone 3 350 - 390 °F
Zone 5 360 - 400 °F
Die Temperature 374 - 410 °F
Melt Temperature 370 - 410 °FProcessing Temperature
Mold Temperature 77.0 - 150 °F
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 50.0 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Elexar® EL 8730R Thermoplastic Elastomer
Teknor Apex Telcar® TL-1934F Styrenic Thermoplastic Elastomer
Teknor Apex Elexar® EL 1934A Thermoplastic Elastomer
Teknor Apex Elexar® EL 1934F Thermoplastic Elastomer
Teknor Apex ELEXAR® EL 8451 Thermoplastic Elastomer

PTEKNP567 / 129640

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.