MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Lucas-Milhaupt BRAZE 300 Silver Based Cadmium Free Filler Metal
Categories: Metal; Nonferrous Metal; Copper Alloy; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes:

Characteristics: Braze 300 is an intermediate temperature silver brazing alloy with a fairly long (160EF/70EC) melting range. This long melting range is helpful when wide gap joints are brazed and is useful in producing large joint fillets to reduce the notch effect in stressed assemblies. Where the higher brazing temperature and characteristics of this alloy are permissible, the lower silver content affords a saving. Handy Flux should be used with this alloy.

Applications:Braze 300 is a good general purpose, intermediate temperature brazing alloy for use on copper, brass, nickel-silver, bronze, steel and other nonferrous alloys melting above 1450EF (765EC). Uses include the brazing of nickel-silver hollow knife handles and electrical equipment. It is particularly adaptable to metal bath dip brazing of fine wires for radio, small transformer and electronics assemblies because its flow point matches the fluid temperature of borax. Borax is used as a metal bath flux cover because it is less corrosive to ceramic pot linings than Handy Flux. Braze 300 exhibits better stability than lower melting alloys when used for metal bath dip brazing.

Specifications:This alloys conforms to the following specifications-AWS A5.8 BAg-20, ASME Boiler & Pressure Vessel Code Sec II-C, SFA-5.8 BAg-20

Information provided by Lucas-Milhaupt, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.84 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 30000 - 35000 psiCopper butt joint
 35000 - 40000 psiNickel-Silver butt joint
 35000 - 45000 psiBrass butt joint
Elongation at Break 7.0 - 17 %% in 2", Nickel-Silver butt joint
 15 - 25 %% in 2", Copper butt joint
 16 - 31 %% in 2", Brass butt joint
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000685 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Melting Point 1250 - 1410 °F
Solidus 1250 °FMelting Point
Liquidus 1410 °FFlow Point
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 37 - 39 %
Other, total <= 0.15 %
Silver, Ag 29 - 31 %
Zinc, Zn 31 - 33 %
 
Descriptive Properties
ColorLight Yellow
Corrosion Resistance1115.5 Mgs/dcm2/Day5% Sulfuric Acid Solution, 160°F, Constant Immersion
 13.9 Mgs/dcm2/Day20% Sulfuric Acid Solution, Room Temperature, Constant Immersion
 15.57 Mgs/dcm2/Day5% Sulfuric Acid Solution, Room Temperature, Constant Immersion
 15.7 Mgs/dcm2/Day10% Sulfuric Acid Solution, Room Temperature, Constant Immersion
 181.1 Mgs/dcm2/Day20% Sulfuric Acid Solution, 160°F, Constant Immersion
 207.6 Mgs/dcm2/Day10% Sulfuric Acid Solution, 160°F, Constant Immersion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NLUCMI20 / 18087

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.