MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical PA930 Processing aid  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Ultra high molecular weight

Application: Foam, soft product etc

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/cc
Bulk Density >= 0.370 g/ccLSY-QB-KD019
Volatiles <= 1.0 %ISO 1625
Particle Mesh Size 35 Mesh<2% (mesh on); LSY-QB-KD018
 200 Mesh<2% (mesh pass); LSY-QB-KD018
Viscosity Measurement 5.7 - 6.6ISO 3105
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 132 °C
Flash Point 490 °C
 
Descriptive Properties
Foreign Material<3% (10 x 10 cm)LSY-QB-KD005
Fusion time40-80 secISO 8130-6

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical PA910 Processing aid
LG Chemical PA828 Processing aid
LG Chemical EH910 PMMA, General Purpose Grade for Extrusion
LG Chemical EG920 PMMA, General Purpose Grade for Extrusion

PLAY726 / 148736

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.