System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Akro-Plastic Akromid® B3 1 black (2501) PA 6 Dry, Heat Stabilized
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, Heat Stabilized
Material Notes:
Description: AKROMID B3 1 black (2501) is an unreinforced, heat stabilized polyamide 6. Applications are engineering parts like fasteners, clips, plugs and caps.
Additive: Heat Stabilizer
Features:
Heat Stabilized
Uses:
Caps
Fasteners
Information provided by Akro-Plastic GmbH
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.13
g/cc
ISO 1183
Moisture Absorption
2.6 - 3.4 %
@Temperature 70.0 °C
Humidity, 62% RH; ISO 1110
Water Absorption at Saturation
9.0 - 10 %
ISO 62
Linear Mold Shrinkage, Flow
0.011
cm/cm
ISO 294-4
Linear Mold Shrinkage, Transverse
0.0095
cm/cm
ISO 294-4
Spiral Flow
107
cm
Cross section: 7 mm x 3.5 mm
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
85.0
MPa
50 [mm/min]; ISO 527-2
Elongation at Break
20 %
50 [mm/min]; ISO 527-2
Tensile Modulus
3600
MPa
1 [mm/min]; ISO 527-2
Flexural Strength
120
MPa
2 [mm/min]; ISO 178
Flexural Modulus
3100
MPa
2 [mm/min]; ISO 178
Charpy Impact Unnotched
NB
@Temperature -30.0 °C
ISO 179/1eU
NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched
2.00
kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
5.00
kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+13
ohm-cm
IEC 60093
Surface Resistance
1.00e+12
ohm
IEC 60093
Comparative Tracking Index
600
V
Solution A; IEC 60112
Thermal Properties
Original Value
Comments
Melting Point
220
°C
DIN EN 11357-1
Deflection Temperature at 0.46 MPa (66 psi)
180
°C
Unannealed; ISO 75/B
Deflection Temperature at 1.8 MPa (264 psi)
60.0
°C
Unannealed; ISO 75/A
Flammability, UL94
V-2
@Thickness 1.60 mm
Glow Wire Ignition Temperature
675
°C
@Thickness 1.60 mm
IEC 60695-2-13
Glow Wire Flammability Index
750
°C
@Thickness 1.60 mm
IEC 60695-2-12
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Akro-Plastic Akromid® B3 1 natural (2499) PA 6 Dry, Heat Stabilized
A. Schulman COMTUF® 464 Glass Reinforced Impact Modified PBT Alloy
Copper, Mill-Hardened UNS C17410, 1/2 HT
Envalior Akulon® F136 PA6, Very High Viscosity, Film Extrusion
Silberline SparkleBrite™ 270NL-PA
PAKRO235 / 182822
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.