MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Sika Sikaflex® Crack Flex Sealant High performance, textured, self-leveling, 1-part polyurethane sealant for sealing cracks.
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Sikaflex Crack Flex Sealant is a single component, textured, self-leveling, premium grade polyurethane sealant for permanently sealing horizontal cracks.

Where to Use: Sikaflex Crack Flex Sealant is used to seal horizontal cracks up to 1" wide in concrete and cementitious slabs, such as:

  • Driveways
  • Garages
  • Sidewalks
  • Balconies
  • Pavements
  • Terraces
  • Decks
  • Walkways
  • Steps
Advantages:
  • 1-component, no mixing, ready-to-use
  • Self-leveling
  • Textured to blend with concrete surface
  • Elastic technology allows for crack movement
  • Waterproof
  • Resists aging and weathering
  • Convenient; use with standard caulk gun

Information provided by Sika Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 76.7 °C170 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 4.44 - 37.8 °C40.0 - 100 °FApplication Temperature
Cure Time 4320 - 7200 min72.0 - 120 hourFinal cure
Tack-Free Time 60.0 - 120 min1.00 - 2.00 hour
Shelf Life 12.0 Month
@Temperature 4.00 - 35.0 °C
12.0 Month
@Temperature 39.2 - 95.0 °F
in original unopened cartridge
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sika Sikaflex® Mortar Fix One-component, polyurethane sealant
Sika SikaBond® Universal One part advanced polyurethane, elastomeric, adhesive

PSIKA927 / 209834

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.