MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ter Hell Plastic Terez® ABS 3320 A UV Acrylonitrile Butadiene Styrene
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: Rapid flowing ABS with high impact strength, antistatic agent and UV stabilizer.

Application: For all kinds of injection molding thin-walled parts.

Information provided by Ter Hell Plastic GMBH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccISO 1183
Water Absorption 0.95 %ISO 62
Melt Flow 34 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 60.0 MPadry; ISO 527
Tensile Strength, Yield 44.0 MPadry; ISO 527
Elongation at Break 12 %dry; ISO 527
Elongation at Yield 2.4 %dry; ISO 527
Tensile Modulus 2300 MPadry; ISO 527
Charpy Impact Unnotched 125 kJ/m²dry; ISO 179
Charpy Impact, Notched 19.0 kJ/m²dry; ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmIEC 60093
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °CISO 75
Vicat Softening Point 95.0 °CB/50; ISO 306
Flammability, UL94 HB
@Thickness 3.20 mm
 
Processing PropertiesOriginal ValueComments
Drying Temperature 80.0 °C
Dry Time 2 - 4 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cheng Yu Plastic VH826 Flame Retardant ABS, Medium Impact
Cheng Yu Plastic VH825 Flame Retardant ABS, Medium Impact
Cheng Yu Plastic VH823 Flame Retardant ABS, High Impact
Avient Stat-Tech™ AS-08CF/000 UV FR V0 Acrylonitrile Butadiene Styrene (ABS)
Henkel Acheson™ SS 24600 Conductive Resin

PTERH916 / 120654

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.