MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Phillips 66 Syncon® WTL ISO Grade 320
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Syncon WTL is a state-of-the-art, synthetic, extreme-pressure (EP) gear lubricant specifically developed for the lubrication of heavily loaded gears and rolling-element bearings in gearboxes on older and new-generation wind turbine generators. Syncon WTL is formulated with synthetic polyalphaolefin (PAO) base oils, a non-chlorinated extreme-pressure additive package and select inhibitors. It has outstanding oxidation resistance and thermal stability at high temperatures to minimize deposit formation and provide long service life. It also has outstanding low-temperature fluidity for use over a wide temperature range. The advanced additive technology provides high load-carrying capacity for outstanding protection against scuffing and wear, as well as excellent protection against rust and corrosion.

Applications:

  • Gear drives of wind turbine generators
  • Enclosed industrial gear drives operating under severe-service conditions, such as heavy loads or high operating temperatures, or in extreme temperature environments
  • Applications where the equipment manufacturer specifies a synthetic AGMA 6 EP gear oil
Syncon WTL meets or exceeds the requirements of the following industry specifications:
  • ANSI/AGMA Standard 9005-E02
  • ANSI/AGMA/AWEA 6006-A03
  • DIN 51517 Part 3, Lubricating Oils, Type CLP
  • ISO 12925-1, Type CKD
Syncon WTL is approved for use in Flender gear units under their specification of 06.12.2005.Features/Benefits:
  • Outstanding performance in wind turbine generator gearboxes
  • Outstanding oxidation resistance and thermal stability at high temperatures
  • Very high load-carrying capacity for protection against scuffing and wear
  • Excellent protection against micropitting
  • Protects against rust and corrosion
  • Non-chlorinated additive system
  • Outstanding low-temperature properties
  • High viscosity index and low pour point for year-round use

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.862 g/cc
Density 7.18 lb/gal
Viscosity Measurement 154Index
Saybolt Viscosity at 100°F 1660 SUS
Saybolt Viscosity at 210°F 170 SUS
Kinematic Viscosity at 40°C (104°F) 320 cSt
Kinematic Viscosity at 100°C (212°F) 34.9 cSt
ASTM Color 1.5ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.83[mg KOH/g]; ASTM D974
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 250 kgASTM D2596
Four Ball Wear 0.350 mmScar Diameter; ASTM D4172
Timken Test 95.0 lbOK Load; ASTM D2782
 
Thermal PropertiesOriginal ValueComments
Pour Point -45.0 °C
Flash Point 246 °CCOC
 
Descriptive Properties
Copper Corrosion1aASTM D130
FZG Micropitting Test>10 Fail StageFVA 51/11 @ 90°C
FZG Scuffing Test>14 Failure Load StageASTM D5182

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5105 / 198358

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.