MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Trelleborg Emerson & Cuming Stycast® 2754 Two-Component Epoxy Flexible Low-Stress Encapsulant
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced; Epoxy, Thermally Conductive

Material Notes: Emerson & Cuming 2754 Stycast® Two-Component Epoxy Flexible Low-Stress Encapsulant
Description

Electronic embedment and sealing of metals, ceramics, and plastics. Protection of stress sensitive components where shock and impact resistance are required. Typical applications include transformers, motors, coils, and other electrical devices

Features
  • Thermally Conductive
  • Good Chemical Resistance
  • Filled
  • Mix Ratio (by weight) = 100:40
Cure Type: Room Temp or Heat Bonding Type: Epoxy

The Stycast® product line is now a part of Henkel; this specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.53 g/cc
Viscosity 24000 cP
@Temperature 25.0 °C
Mixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.9
@Frequency 1e+6 Hz
Dielectric Strength 450 V/mil
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.630 W/m-K
Maximum Service Temperature, Air 105 °C
Minimum Service Temperature, Air -65.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time >= 2.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cotronics Duralco™ 125 450°F Stress Free, Silver Filled Epoxy, Thermally Conductive
Celanese CoolPoly® D5112 Thermally Conductive Polyphenylene Sulfide
Celanese CoolPoly® D3612 Thermally Conductive Polyamide (PA66/6)
Celanese CoolPoly® D5502 Thermally Conductive Liquid Crystalline Polymer
Celanese CoolPoly® D5506 Thermally Conductive Liquid Crystalline Polymer

PEMERS03 / 35695

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.