(Viewing data as-entered.
Click here
to return)
Eurofoam Porocell POR 301/B NR-SBR Foam
Categories:
Polymer
;
Thermoset
;
Rubber or Thermoset Elastomer (TSE)
;
Styrene Butadiene Rubber
Material Notes:
Natural and styrene butadiene rubber foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; gaskets.
Information provided by Eurofoam s.r.l.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.100
-
0.140
g/cc
Water Absorption
<= 5.0 %
Mechanical Properties
Original Value
Comments
Hardness, Shore OO
50 - 60
Elongation at Break
>= 300 %
Compressive Yield Strength
0.0550
MPa
@Strain 25 %
Tear Strength
0.620
kN/m
Compression Set
20 %
@Strain 50 %
Thermal Properties
Original Value
Comments
Maximum Service Temperature, Air
80.0
°C
Minimum Service Temperature, Air
-50.0
°C
Descriptive Properties
Cellular Structure
Closed
Color
Black
Vulcanization
Peroxide
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Garlock 2920 Compressed Aramid Fiber Gasketing, SBR Binder
Eurofoam Porocell POR 301/B HD 300 NR-SBR Foam
INEOS Styrolution Styrolux® BX6400 SBC
Garlock SBR Extruded Skirtboard
Dow SE SLR-6410 Solution polymerized Styrene Butadiene Rubber (S-SBR)
PEUROF952 / 198182
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.