MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem FC31D LLDPE Blown Film Extrusion Polyethylene Copolymer  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Butene, Film

Material Notes: The FC31D resin is a linear low-density polyethylene, copolymer of butene -1, produced by the solution process for blow film extrusion. It has excellent mechanical properties, especially hot tack. It contains processing aid, antiblock, slip, and antioxidant additives. Its applications include: general purpose pure or blends; and laminating and automatic packaging of solids and liquids. Recommended Processing Conditions: Pure - The FC31D resin should processed on specific extruders for LLDPE. The best results are obtained at a melt temperature within the range of 200 to 220ºC. Recommended blow up ratio: 1.8 to 3.0:1. Blends - The FC31D resin can be processed with LDPE on conventional extruders with a maximum ratio of 30%. The best results are obtained with polyethylene resins of low melt index. The recommended temperature profile for blends with LDPE is slightly higher than those ones for the conventional LDPE (10 to 20ºC).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.919 g/ccASTM-D792
Melt Flow 0.75 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM-D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 880 %ASTM-D882
Film Elongation at Break, TD 1150 %ASTM-D882
Elmendorf Tear Strength MD 150 gASTM-D1922
Elmendorf Tear Strength TD 430 gASTM-D1922
Elmendorf Tear Strength, MD 6.00 g/micronASTM-D1922
Elmendorf Tear Strength, TD 17.2 g/micronASTM-D1922
Dart Drop 4.80 g/micronASTM-D1709
Dart Drop Test 120 gASTM-D1709
Film Tensile Strength at Break, MD 30.0 MPaASTM-D882
Film Tensile Strength at Break, TD 30.0 MPaASTM-D882
1% Secant Modulus, MD 170 MPaASTM-D882
1% Secant Modulus, TD 190 MPaASTM-D882
 
Optical PropertiesOriginal ValueComments
Haze 7.0 %ASTM-D1003
Gloss 95 %Angle 60°; ASTM-D2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips 6109FK Linear low density polyethylene blown film resin
Braskem TI4015F Impact Copolymer Polypropylene
Braskem TI4007G Impact Copolymer Polypropylene
Braskem TI4003F Impact Copolymer Polypropylene
Braskem TI2150C High Crystallinity Copolymer Polypropylene

PBRAS842 / 106688

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.