MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco Aremco-Bond™ 631 High Performance Epoxide
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: Clear-Amber, 1:1, Good Bond Strength and Corrosion Resistance.
Also available filled with aluminum oxide (Alumina) or pigments.

Vendors: Aremco’s High Performance Epoxies provide a wide range of solutions for bonding ceramics, composites, glass, metals, plastics, and other materials. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/cc
Viscosity 25000 cPMixed Viscosity
Linear Mold Shrinkage 0.0020 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75
Flexural Strength 10200 psiASTM D790
Shear Strength 3000 psiASTM D1002-94
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.20e+14 ohm-cm
Dielectric Constant 3.12
@Frequency 1000 Hz
Dielectric Strength 440 V/mil
Dissipation Factor 0.010
 
Thermal PropertiesOriginal ValueComments
CTE, linear 27.0 µin/in-°F
@Temperature 20.0 °C
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -85.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 93.3 °C
Recommended Cure
 24.0 - 48.0 hour
@Temperature 23.0 °C
at RT, Alternate Cure
Pot Life 240 min
@Temperature 25.0 °C
100 gm mass
 
Descriptive Properties
Chemical ResistanceGood
ColorAmber
Mix Ratio by Weight1:1resin:hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Thermal Ceramics K-Bond (wet, air setting) Mortar
Abatron AboCast 8504-5 One-Component Epoxy
Abatron AboCast 7802-1/AboCure 7804-3 (40 pbw) Epoxy
Devcon High-Performance Backing Compound Epoxy
BCC Products BC 7009-1 Epoxy Casting

PAREM04 / 24268

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.