MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

SunChemical Gwent D2070209P6 White Dielectric Paste
Categories: Fluid; Other Engineering Material; Ceramic/Metallic Coating; Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low temperature formation of a thermosetting polymer. This ink has excellent adhesion, chemical and environmental resistance properties.
Excellent adhesion to ITO, chemical and environmental resistance.
Screen Printing Equipment: semi-automatic, manual
Screen Types: stainless steel, polyester, mesh 156-325tpi
Substrate: ITO coated polyester

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 73.5 - 76.5 %
@Temperature 150 °C
73.5 - 76.5 %
@Temperature 302 °F
Viscosity 1400 - 2300 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
1400 - 2300 cP
@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Thickness 20.0 microns0.787 milDouble layer on 175µm ITO coated polyester
Storage Temperature 20.0 °C68.0 °Fsealed container
 
Processing PropertiesMetricEnglishComments
Cure Time  3.00 min
@Temperature 130 °C
0.0500 hour
@Temperature 266 °F
belt dryer
 10.0 min
@Temperature 130 °C
0.167 hour
@Temperature 266 °F
box oven
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Coverage cm2/g2421st layer, Using a 230 mesh stainless steel screen
 2602nd layer, Using a 230 mesh stainless steel screen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SunChemical Gwent C2110817D5 Conductive Silver Polymer Paste
SunChemical Gwent R2070613P2 Resin Binder
SunChemical Gwent D2020409D8 Dielectric for Stainless Steel
SunChemical Gwent C2110127D3 Nanocopper based Paste
SunChemical Gwent C2100211D1 Silicone Based Silver Paste

WGELZ9047 / 139360

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.