MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sanyo PELESTAT® NC6321 ABS (12wt%)
Categories: Polymer; Thermoplastic

Material Notes: PELESTAT® alloy type anti-static additives are true IDP (Inherent Dissipative Polymers) that give permanent static dissipation performance to thermoplastics. Pelestat® comes tailored to a variety of thermoplastics like polyolefins, ABS, PC/ABS, PS, HIPS, Acetal Nylon, PBT, PTEG, etc. Pelestat® is not affected by moisture or humidity and offers the highest heat resistance of any anti-stats without affecting mechanical properties of the thermoplastic.

Information provided by Tomen America, a US distributor of Pelestat.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 30 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 41.0 MPa
Flexural Modulus 2.20 GPa
Izod Impact, Notched 140 J/m
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 2.00e+11 ohm
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 192.2 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sanyo PELESTAT® NC6321 Antistatic Additive
Sanyo PELESTAT® NC7530 Antistatic Additive
Sanyo PELESTAT® 300 Antistatic Additive
Sanyo PELESTAT® 2450 Antistatic Additive
Arkema Pebax® MV 1074 SP 01 Polyether Block Amide (PEBA)

PSANYO05 / 66529

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.