System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Eagle Brass 725 Copper Nickel Tin, Extra Spring
Categories:
Metal
;
Nonferrous Metal
;
Copper Alloy
Material Notes:
Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap terminals.
Information provided by Eagle Brass Company
Key Words:
UNS C72500, ASTM B122
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.321
lb/in³
Annealed
Mechanical Properties
Original Value
Comments
Hardness, Rockwell 30T
75 - 80
Thickness > 0.020 Inch
Tensile Strength, Ultimate
90.0
-
105
ksi
Tensile Strength, Yield
88.0
-
102
ksi
0.2% offset
Elongation at Break
<= 1.0 %
in 2 in.
Tensile Modulus
20000
ksi
Electrical Properties
Original Value
Comments
Electrical Resistivity
0.0000162
ohm-cm
Annealed
Thermal Properties
Original Value
Comments
CTE, linear
9.20
µin/in-°F
@Temperature 20.0 - 300 °C
Thermal Conductivity
372
BTU-in/hr-ft²-°F
Component Elements Properties
Original Value
Comments
Copper, Cu
88.2 %
Nickel, Ni
9.5 %
Tin, Sn
2.3 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Materion BrushForm® 96 Copper-Nickel-Tin Mill Hardened Strip (UNS C72700), TM00
Geon® Performance Solutions Synplast™ 701P-N Di (C7-C11 Alkyl) Phthalate
Materion BrushForm® 158 Copper-Nickel-Tin Mill Hardened Strip (UNS C72900), TM10
Materion BrushForm® 96 Copper-Nickel-Tin Mill Hardened Strip (UNS C72700), TM04
Materion BrushForm® 158 Copper-Nickel-Tin Cold Rolled Strip (UNS C72900), EHT (TS08)
NEAGLE192 / 147441
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.