MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Silberline EternaBrite® 651-7
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: EternaBrite® pigments are leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on cornflake geometry and offer enhanced leafing properties in solvent and waterborne flexographic and gravure inks for stronger metallic effects. Although EternaBrite® pigments can be used in aqueous inks they are not treated to protect against the aluminum-water reaction and special care must be taken to evaluate the gassing stability of each grade in the final ink formulation. High or excessive shear during ink production can initiate the aluminum-water reaction. Care must be taken to avoid excessive or high shear during processing when used in ink formulations containing water.

Applications: Printing Inks

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.62 g/cc
Volatiles 28 %
Particle Size 7.0 µm
 
Descriptive Properties
CategoryLeafing
SolventsInk Oil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Type 431 Martensitic Stainless Steel, Intermediate Temper Forgings, UNS S43100
Type 431 Martensitic Stainless Steel, Hard Temper Forgings, UNS S43100
Overview of materials for Bronze
MetalTek WC 6 Cast UNS J24054 Alloy Steel
Low-silicon bronze B, UNS C65100, OSO35 Temper rod

ESIBER246 / 6001

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.