MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Desmodur® BL 5375 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Blocked aliphatic polyisocyanate based on H12MDI. In combination with hydroxyl-bearing polyols, especially Desmophen® grades, to formulate lightfast one-component polyurethane stoving coatings; as an additive in conventional stoving systems to improve adhesion and flexibility.

Properties / Applications: Desmodur® BL 5375 was developed as a hardener component for lightfast one-compnent stoving polyurethane systems. As with air-drying two-component PU coatings, the film properties can be influenced by the crosslinking density and the selection of hydroxyl-bearing polyol co-reactant. Desmodur® BL 5375 can be used to formulate high-quality industrial finishes, especially for coil and can coating. The product can also be used as an additive to improve flexibility, tear resistance and adhesion of conventional stoving coil and can coating systems. The combination of Desmodur® BL 5375 with Desmophen® 670 results in particularly high flexibility. Such a formulation is suitable for tear resistance coatings flexible substrates and those vulnerable to impact. Available results form Florida weathering tests show that Desmodur® BL 5375 has good weather stability comparable with that of Desmodur® BL 3175.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccDIN 53 217/3
Volatiles 23 - 27 %0.5 g/60 min/60 °C; DIN EN ISO 3251
Viscosity 2500 - 5500 cPDIN EN ISO 3219/A.3
 
Thermal PropertiesOriginal ValueComments
Flash Point 48.0 °CDIN 53 513/1
 
Descriptive Properties
Color<150Hazen, DIN EN 1557
Content8.9%NCO content, blocked

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Platilon® M2234 Polyether-Blockamide Film
Precision Polymer Engineering Q90Y Polyurethane Rubber
Precision Polymer Engineering Q90A Polyurethane Rubber
Precision Polymer Engineering Q70Y Polyurethane Rubber
Precision Polymer Engineering Q65B Polyurethane Rubber

PCOVEST0332 / 202115

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.