System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Network Polymers NPP 30-0200 TF20
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene with 20% Talc Filler
Material Notes:
Description:
20% Talc Filled Homopolymer Polypropylene
Information provided by Network Polymers Inc.
A. Schulman has acquired Network Polymers.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.06
g/cc
ASTM D792
Melt Flow
2.0
g/10 min
@Load 2.16 kg,
Temperature 230 °C
Procedure A Condition L; ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Shore D
77
ASTM D2240
Tensile Strength, Yield
5300
psi
2 in per min, tangent; ASTM D638
Flexural Modulus
390000
psi
Test Method I, Procedure B (chs speed 0.05 in/min), Tangent; ASTM D790
Izod Impact, Notched
0.800
ft-lb/in
ASTM D256
0.500
ft-lb/in
@Temperature -30.0 °C
ASTM D256
Gardner Impact
4.00
ft-lb
ASTM D3029
Thermal Properties
Original Value
Comments
Deflection Temperature at 0.46 MPa (66 psi)
123
°C
ASTM D648
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Aclo Accutech Polypropylene HP0335T40V Homopolymer Talc Reinforced
TIMCAL TIMREX® PP 25 Natural Flake Graphite
Aclo Accuguard Polypropylene CP1467V2CSL Copolymer Flame Retardant Copper Stabilized
Aclo Accuguard Polypropylene CP0467V2CSL Copolymer Flame Retardant Copper Stabilized
Aclo Accuguard Polypropylene CP0467V0CSV Copolymer Flame Retardant Automotive Approved grade
PDIAM076 / 29914
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.