Product description: Grivory GV-4 FWA black 9225 is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide. Grivory GV-4 FWA black 9225 is used for injection molding technical parts, exhibiting exceptional characteristics even after moisture absorption:- high stiffness and strength
- dimensional stability, low warpage
- good chemical resistance
- good surface finish
Grivory GV is the economical alternative to die-cast alloys. Grivory GV-4 FWA black 9225 is a specially heat stabilized material. It is particularly suitable for parts in direct contact with drinking water and food. Grivory GV-4 FWA black 9225 is suitable for all engineering thermoplastic applications with the requirement of approvals in contact with foodstuffs or/and in contact with drinking water.Information provided by EMS Grivory |