MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

Plansee DENSIMET® D2M Tungsten-Nickel-Molybdenum-Iron Alloy
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: Characteristics:
  • Easy processing
  • High density
  • Precision forming and machining
  • High ductility
  • High strength
  • 100 % impermeable

Typical Applications:

    Balancing weights in motors and drive components
  • Vibration dampers in motors and drive components
  • Collimator and shielding components for X-ray and gamma radiation protection
  • Aviation and aerospace: propeller and helicopter blades
  • Sports equipment: golf clubs
  • Optical industry: microscopes and measuring instruments

Information provided by Plansee.

Vendors: PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 16.9 - 17.6 g/cc0.611 - 0.636 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 300 - 360300 - 360HV10
Tensile Strength >= 800 MPa>= 116000 psi
Tensile Strength, Yield >= 550 MPa>= 79800 psi
Elongation at Break >= 4.0 %>= 4.0 %
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.30 µm/m-°C2.94 µin/in-°F
Thermal Conductivity 65.0 W/m-K
@Temperature 500 °C
451 BTU-in/hr-ft²-°F
@Temperature 932 °F
Maximum Service Temperature, Air 600 °C1110 °FOxidation Resistance
 
Component Elements PropertiesMetricEnglishComments
Ni, Fe, Mo 10 %10 %
Tungsten, W 90 %90 %
 
Descriptive Properties
Ductilitymuch greater than pure W
Fineness of Graingreater than pure W
Machinability/Workabilitymuch greater than pure W

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plansee DENSIMET® D170 Tungsten-Nickel-Iron Alloy
Plansee DENSIMET® D185 Tungsten-Nickel-Iron Alloy
Plansee DENSIMET® D188 Tungsten-Nickel-Iron Alloy
Plansee DENSIMET® D176 Tungsten-Nickel-Iron Alloy
Astaras ANVILOY® 1150 Tungsten Based High Temp Alloy

NPLAM943 / 135499

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.