MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Shakespeare Isocor™ TT25TI Nylon 6 Terpolymer
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Isocor™ is a low viscosity nylon terpolymer. Isocor™ TT25TI is useful as an additive for improved impact in phenolics, polyesters, urethanes and nylons. The unique chemistry affords it special dispersion properties in hard to color formulations and can be used as melt adhesive for dissimilar surfaces. Isocor™ TT25TI is soluble in most common alcohols and is used as a thread bonding agent where suppleness, melt point, or solubility is a concern.

Used for color concentrates, impact modifier, melt adhesives, thread bonding.

Information provided by Shakespeare Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.092 g/ccASTM D 792
Viscosity Measurement 20 - 30Relative Viscosity; ASTM D789-97
 
Thermal PropertiesOriginal ValueComments
Softening Point 140 °CTest Method not Specified
Glass Transition Temp, Tg 142 °CASTM D 3418-97
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 10B*

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Shakespeare Isocor™ TT65SI Nylon 6 Terpolymer
Shakespeare Isocor™ 651 Nylon 6 Terpolymer
Shakespeare Isocor™ 637 Nylon 6 Terpolymer
Celanese Butoxyl® 50000872 3-Methoxy-n-Butylacetate

PSHAKE102 / 67381

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.