MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Dyneon™ PFA 6515NZ Perfluoroalkoxy Fluorothermoplastic
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA)

Material Notes: PFA designed for higher speed or higher shear processing such as injection molding and wire insulation. Demonstrates universal chemical and solvent resistance, high dielectric strength, excellent weathering, flame resistance and a wide service range of temperature resistance.

Features and Benefits:

  • Service temperatures up to 260°C (500°F).
  • Excellent universal resistance to solvents and chemicals.
  • Excellent weatherability.
  • Excellent electrical properties.
  • High light transmission.
  • High limiting oxygen index: Does not support combustion.
  • Extremely smooth surfaces.
  • Non-stick characteristics.
  • Good low-friction properties.
Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Index of Compound 15 g/10 min
@Load 5.00 kg,
Temperature 372 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 26.0 MPa
Flexural Modulus 0.620 GPa
 
Thermal PropertiesOriginal ValueComments
Melting Point 310 °C
Maximum Service Temperature, Air 260 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Dyneon™ PFA 6515 UHPZ Perfluoroalkoxy Fluorothermoplastic Granules
3M Dyneon™ PFA 6502 UHPZ Perfluoroalkoxy Fluorothermoplastic Granules
3M Dyneon™ PFA 6502 TAZ Perfluoroalkoxy Fluorothermoplastic Granules
Syensqo (Solvay Specialty Polymers) Hyflon® PFA P7310 Perfluoroalkoxy (PFA)
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded

PDYNE012_a / 149076

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.