MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Danquinsa DANCURE® 246-06 Isocyanate Hardeners
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DANCURE® 246-06 is a very reactive isocyanate hardener which is free of chlorinated hydrocarbon solvents and in most cases tri functional and of a light colored aspect. DANCURE® 246-06 is solved in ethyl acetate and is applied for the curing of polyurethane-, polychloroprene- and natural rubber adhesives.

Application: DANCURE® 246-06 is added to adhesives, sealants and coating compounds in order to improve the resistances against high and low temperature, chemicals and hydrolysis. In case of metallic surfaces, DANCURE® 246-06 can be used as a surface primer for a later coating or bonding.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.990 g/cc0.0358 lb/in³DIN 51.757
Solids Content 27.5 - 29.5 %27.5 - 29.5 %DIN 53.189
Brookfield Viscosity 5.0 - 10 cP5.0 - 10 cPRVT
 
Thermal PropertiesMetricEnglishComments
Flash Point -6.00 °C21.2 °FDIN 51.755
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 9.0<= 9.01933
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Aspectlightly yellowish liquid
Composition5.8-6.2%NCO
SolventEthyl acetate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDANQ107 / 294527

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.