IPETHENE® 323 is a general purpose low density polyethylene film extrusion grade. It contains a high level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between mechanical and optical properties. APPLICATIONS IPETHENE® 323 is mainly used for the production of 25 to 80 µm films for the applications of general purpose films, Form-Fill-Seal packaging, and packaging of textile products. |