MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Asahi Kasei ASACLEAN PX2 Purging Compound
Categories: Polymer; Thermoplastic; Purging Compound

Material Notes: ASACLEAN PX2 Grade excels in purging super-engineering resins at processing temperatures of up to 420°C (790°F). PX2 Grade is the most powerful high temperature grade for cleaning hard-to-clean resins. PX2 Grade generates low levels of smoke and odor across the entire operating temperature range of 280°C to 420°C (535°F to 790°F)

Information provided by Asaclean.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Processing Temperature 280 - 420 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Asahi Kasei ASACLEAN E Purging Compound
AGC Lumiflon LF-910LM Solvent Soluble Fluoropolymer
PTS Trimid® N6-G30L 30% GFR Lubricated Nylon 6
Mitsubishi Chemical Advanced Materials Nylatron® MD PA6, Metal-detectable Nylon (ASTM Product Data Sheet)
Ipiranga Petrochem MB 0434 LS-L MDPE

PACLEAN08 / 175999

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.