MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zinc Zn-Cu-Ti Alloy (Zn-0.8Cu-0.15Ti), Cold-Rolled - Transverse Properties
Categories: Metal; Nonferrous Metal; Zinc Alloy

Material Notes: Hot Work Temperature 150-300°C

Properties vary with rolling direction. Average values and values for longitudinal direction are listed separately.

Key Words: UNS Z41320
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.17 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 80500 kg load; 10 mm hardened steel ball
Hardness, Knoop 103Estimated from Brinell Value
Hardness, Rockwell B 49Estimated from Brinell Value
Hardness, Vickers 90Estimated from Brinell Value
Tensile Strength, Ultimate 260 MPa
Elongation at Break 44 %in 5 cm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000624 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 19.4 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.402 J/g-°C
Thermal Conductivity 105 W/m-K
Melting Point 419 - 422 °C
Solidus 419 °C
Liquidus 422 °C
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 250 °C45 minutes
Hot-Working Temperature 150 - 300 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.0010 %
Cadmium, Cd <= 0.050 %
Copper, Cu 0.50 - 1.5 %
Iron, Fe <= 0.012 %
Lead, Pb <= 0.10 %
Tin, Sn <= 0.0010 %
Titanium, Ti 0.12 - 0.50 %
Zinc, Zn 97.836 - 99.38 %As balance; per ASTM B 69

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zinc Zn-Cu-Ti Alloy (Zn-0.8Cu-0.15Ti), Cold-Rolled - Longitudinal Properties
Zinc Zn-Cu-Ti Alloy (Zn-0.8Cu-0.15Ti), Hot-Rolled - Longitudinal Properties
Zinc Zn-Cu-Ti Alloy (Zn-0.8Cu-0.15Ti), Hot-Rolled - Transverse Properties
Zinc Zn-Cu-Ti Alloy (Zn-0.8Cu-0.15Ti), Hot-Rolled
Silver-Copper Eutectic Alloy (72Ag-28Cu; UNS P07720; AWS BAg-8), 10% Cold Work

MZN553 / 14532

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.