MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 4201 TFE 5 Thermoplastic Polyimide (TPI), Glass Fiber - PTFE Lubricated
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Glass Fiber

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/ccASTM D 792
Filler Content 10 %Primary Additive
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 17000 psiASTM D 638
Elongation at Break 4.0 - 6.0 %ASTM D 638
Tensile Modulus 750 ksiASTM D 638
Flexural Strength 25000 psiASTM D 790
Flexural Modulus 700 ksiASTM D 790
Izod Impact, Notched 1.50 ft-lb/in
@Thickness 3.17 mm
D 256
Izod Impact, Unnotched 17.0 ft-lb/in
@Thickness 3.17 mm
ASTM D4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmASTM D 257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 550 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.59 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 750 - 780 °F
Mold Temperature 350 - 450 °F
Drying Temperature 400 °F
Dry Time 6 hour
Moisture Content 0.010 %
Dew Point -40.0 °F
Injection Pressure 20000 - 28000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, 40% Glass Fiber Filled
RTP Company RTP 4207 Thermoplastic Polyimide (TPI), Glass Fiber - UL94 V-0
E-Glass Fiber, Generic
Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced

PQZWA3892 / 91794

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.