Characterization: Makrofol PC VM 000000 is an extrusion film based on Makrolon® polycarbonate. Properties / Applications: Makrofol PC VM 000000 is glare free and scratch resistant film. Typical applications are automotive, labels, control panels, membrane switches, nameplates, light diffusion, packaging and automotive interior decoration. Makrofol PC VM 000000 is available in various standard thicknesses from 0.005 ” to 0.030 ” (125 microns to 750 microns). Other thicknesses are available on request. The surface combination of Makrofol PC VM 000000 is one side velvet and one side matte. As with any product, use of Makrofol PC VM 000000 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability. Information provided by Covestro |