MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
Categories: Polymer; Thermoplastic; Polystyrene (PS); Syndiotactic Polystyrene (SPS); Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 - 1.54 g/ccAverage value: 1.30 g/cc Grade Count:82
Filler Content 10.0 - 40.0 %Average value: 27.9 % Grade Count:55
Water Absorption 0.00900 - 0.0900 %Average value: 0.0125 % Grade Count:31
Moisture Absorption at Equilibrium 0.0100 - 0.450 %Average value: 0.0414 % Grade Count:34
Linear Mold Shrinkage 0.00100 - 0.00900 cm/cmAverage value: 0.00293 cm/cm Grade Count:69
Linear Mold Shrinkage, Transverse 0.00200 - 0.0110 cm/cmAverage value: 0.00580 cm/cm Grade Count:40
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 65.5 - 175 MPaAverage value: 114 MPa Grade Count:77
Tensile Strength, Yield 92.0 - 132 MPaAverage value: 113 MPa Grade Count:19
Elongation at Break 0.600 - 3.00 %Average value: 1.85 % Grade Count:64
Modulus of Elasticity 4.14 - 24.1 GPaAverage value: 9.99 GPa Grade Count:72
Flexural Yield Strength 103 - 250 MPaAverage value: 173 MPa Grade Count:64
Flexural Modulus 4.14 - 24.1 GPaAverage value: 9.85 GPa Grade Count:69
Izod Impact, Notched 0.427 - 1.49 J/cmAverage value: 0.875 J/cm Grade Count:47
Izod Impact, Unnotched 1.44 - 13.3 J/cmAverage value: 4.15 J/cm Grade Count:27
Izod Impact, Notched (ISO) 3.70 - 13.0 kJ/m²Average value: 10.5 kJ/m² Grade Count:36
Izod Impact, Unnotched (ISO) 18.0 - 57.0 kJ/m²Average value: 35.5 kJ/m² Grade Count:35
Charpy Impact Unnotched 2.30 - 6.80 J/cm²Average value: 3.99 J/cm² Grade Count:34
Charpy Impact, Notched 0.800 - 1.40 J/cm²Average value: 1.12 J/cm² Grade Count:34
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+14 - 1.30e+18 ohm-cmAverage value: 4.73e+16 ohm-cm Grade Count:34
Dielectric Constant 2.80 - 3.50Average value: 3.07 Grade Count:35
Dielectric Strength 17.0 - 50.0 kV/mmAverage value: 30.7 kV/mm Grade Count:48
Dissipation Factor 0.000600 - 0.0690Average value: 0.00431 Grade Count:43
Arc Resistance 60.0 - 180 secAverage value: 123 sec Grade Count:26
Comparative Tracking Index 250 - 600 VAverage value: 472 V Grade Count:36
Hot Wire Ignition, HWI 0.000 - 120 secAverage value: 66.1 sec Grade Count:19
High Amp Arc Ignition, HAI 30.0 - 120 arcsAverage value: 117 arcs Grade Count:19
High Voltage Arc-Tracking Rate, HVTR 0.000 - 150 mm/minAverage value: 31.1 mm/min Grade Count:14
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.0 - 42.3 µm/m-°CAverage value: 22.6 µm/m-°C Grade Count:47
 18.0 - 18.0 µm/m-°C
@Temperature 100 - 100 °C
Average value: 18.0 µm/m-°C Grade Count:1
CTE, linear, Transverse to Flow 29.0 - 81.0 µm/m-°CAverage value: 49.1 µm/m-°C Grade Count:33
Deflection Temperature at 0.46 MPa (66 psi) 140 - 270 °CAverage value: 260 °C Grade Count:51
Deflection Temperature at 1.8 MPa (264 psi) 132 - 265 °CAverage value: 229 °C Grade Count:70
Vicat Softening Point 255 - 263 °CAverage value: 262 °C Grade Count:14
UL RTI, Electrical 50.0 - 130 °CAverage value: 86.9 °C Grade Count:28
UL RTI, Mechanical with Impact 50.0 - 120 °CAverage value: 84.1 °C Grade Count:28
UL RTI, Mechanical without Impact 50.0 - 130 °CAverage value: 85.2 °C Grade Count:28
Flammability, UL94 HB - 5VAGrade Count:53
 
Processing PropertiesOriginal ValueComments
Processing Temperature 271 - 327 °CAverage value: 299 °C Grade Count:5
Melt Temperature 270 - 327 °CAverage value: 301 °C Grade Count:63
Mold Temperature 40.0 - 155 °CAverage value: 113 °C Grade Count:68
Drying Temperature 80.0 - 120 °CAverage value: 96.3 °C Grade Count:49
Moisture Content 0.0200 %Average value: 0.0200 % Grade Count:20
Dew Point -28.9 °CAverage value: -28.9 °C Grade Count:20
Injection Pressure 68.9 - 103 MPaAverage value: 86.2 MPa Grade Count:25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Idemitsu Kosan Xarec® D132 SPS, 25% Glass Filled
Overview of materials for Polystyrene, Molded, Unreinforced
Dow Questra® EA503 High Heat Syndiotactic Polystyrene, 30% Glass Filled
Overview of materials for Polystyrene, Extrusion Grade
Overview of materials for Polystyrene, Glass Filled

O4861 / 78422

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.