MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Materion C103 Electrical Contact Alloy
Categories: Metal; Electronic/Magnetic Alloy; Nonferrous Metal; Precious Metal; Palladium Alloy; Silver Alloy

Material Notes: Has excellent conductivity, plus controllable stiffness and hardness. It is compatible with high volume stamping.

Williams Advanced Alloys is now a part of Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 11.8 g/cc
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000313 - 0.0000352 ohm-cm
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 14 %
Gold, Au 10 %
Palladium, Pd 35 %
Platinum, Pt 10 %
Silver, Ag 30 %
Zinc, Zn 1.0 %
 
Descriptive Properties
ASTM Equiv.B540
Compare To:Paliney 7
Tempers AvailableAR,A,WQ

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Materion C105 Electrical Contact Alloy
Copper, Cu; Cold-Worked
Aluminum, Al
Free-Cutting Brass, UNS C36000
Copper, Cu; Cold Drawn

NWILL91 / 19979

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.