MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Petropol Petrotene® A3 T20 PRTA010 PH336 PP, 20% Mineral Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Product Description: 20% Mineral Reinforced, Polypropylene Homopolymer

Applications:

  • PETROTENE A3 T20 PRTA010 PH336 has been developed especially for the automotive industry.
  • Automotive interior/exterior parts
  • Cowl vent grilles
  • Interior trims

    Resin ID (ISO 1043): PP-MD20
    Processing: Injection Molding
    Color: Black

    Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ASTM D792
Water Absorption 0.020 %0.020 %ASTM D570
Linear Mold Shrinkage, Transverse 0.015 cm/cm0.015 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 30.0 MPa4350 psi50 mm/min; ISO 527
Elongation at Break 8.0 %8.0 %ISO 527
Flexural Strength 47.0 MPa6820 psi2 mm/min; ISO 178
Flexural Modulus 1.70 GPa247 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²ISO 180/A
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point  107 °C
@Load 5.10 kg
225 °F
@Load 11.2 lb
50°C/h; ASTM D1525
 157 °C
@Load 1.02 kg
315 °F
@Load 2.25 lb
50°C/h; ASTM D1525
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Processing Temperature 190 - 230 °C374 - 446 °FMolding
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4.00 hour4.00 hour
 
Descriptive Properties
Fogging100°C, 16h, DIN 75201

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPETROPOL264 / 313172

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.